321 Stainless Steel Jalur
Stainless Steel Lambaran Plate Kelas Baogu Supply
Tipe | Kelas | Kelas | Komponén Kimia% | ||||||||||
C | Cr | Ni | Mn | P | S | Mo | Si | Cu | N | Lain | |||
Austenitik | 201 | SUS201 | ≤0.15 | 16.00-18.00 | 3.50-5.50 | 5.50–7.50 | ≤0,060 | ≤0,030 | - | ≤1.00 | - | ≤0.25 | - |
202 | SUS202 | ≤0.15 | 17.00-19.00 | 4.00-6.00 | 7.50-10.00 | ≤0,060 | ≤0,030 | ≤1.00 | - | ≤0.25 | - | ||
301 | 1.431 | ≤0.15 | 16.00-18.00 | 6.00-8.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | ≤0.10 | - | |
304 | 1.4301 | ≤0.07 | 17.00-19.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
304L | 1.4307 | ≤0,030 | 18.00-20.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
304H | 1.4948 | 0.04-0.10 | 18.00-20.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
309 | 1.4828 | ≤0.20 | 22.00-24.00 | 12.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
309S | * | ≤0.08 | 22.00-24.00 | 12.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
310 | 1.4842 | ≤0.25 | 24.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1,50 | - | - | - | |
310S | * | ≤0.08 | 24.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1,50 | - | - | - | |
314 | 1.4841 | ≤0.25 | 23.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | 1.50-3.00 | - | - | - | |
316 | 1.4401 | ≤0.08 | 16.00-18.50 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | - | - | |
316L | 1.4404 | ≤0,030 | 16.00-18.00 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | - | - | |
316Ti | 1.4571 | ≤0.08 | 16.00-18.00 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | 0.1 | Ti5(C+N)~0,70 | |
317 | * | ≤0.08 | 18.00-20.00 | 11.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | 3.00-4.00 | ≤1.00 | - | 0.1 | - | |
317L | 1.4438 | ≤0.03 | 18.00-20.00 | 11.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | 3.00-4.00 | ≤1.00 | - | 0.1 | - | |
321 | 1.4541 | ≤0.08 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Ti5(C+N)~0,70 | |
321H | * | 0.04-0.10 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Ti5(C+N)~0,70 | |
347 | 1.455 | ≤0.08 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Nb≥10*C%-1.10 | |
347H | 1.494 | 0.04-0.10 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Nb≥10*C%-1.10 | |
xm-19 | Nitronik50 | ≤0.06 | 20.50-23.50 | 11.50-13.50 | 4.0-6.0 | ≤0,045 | ≤0,030 | 1.50-3.00 | ≤1.00 | - | 0.2-0.4 | Nb: 0.10-0.30 V: 0.10-0.30 | |
904L | N08904 | ≤0.02 | 19.0-23.0 | 23.0-28.0 | 4.0-5.0 | ≤0,045 | ≤0,035 | ≤1.00 | 0.1 | Cu: 1.0-2.0 | |||
Duplex | 2205 | S32205 | ≤0.03 | 22.0-23.0 | 4.5-6.5 | ≤2.00 | ≤0,030 | ≤0,020 | 3.0-3.5 | ≤1.00 | - | 0.14-0.20 | |
2507 | S32750 | ≤0.03 | 24.0-26.0 | 6.0-8.0 | ≤1.20 | ≤0,035 | ≤0,020 | 3.0-5.0 | ≤0.80 | 0.5 | 0.24-0.32 | ||
* | S32760 | ≤0.03 | 24.0-26.0 | 6.0-8.0 | ≤1.00 | ≤0,030 | ≤0,010 | 3.0-4.0 | ≤1.00 | 0.5-1.00 | 0.2-0.3 | ||
2304 | S32304 | ≤0.03 | 21.5-24.5 | 3.0-5.5 | ≤2,50 | ≤0,040 | ≤0,030 | 0.05-0.6 | ≤1.00 | 0.05-0.6 | 0.05-0.2 | ||
329 | 1.446 | ≤0.08 | 23.00-28.00 | 2.00-5.00 | ≤1.00 | ≤0,040 | ≤0,030 | 1.00-2.00 | ≤0.75 | - | - | ||
Ferrite | 409 | S40900 | ≤0.03 | 10.50-11.70 | 0.5 | ≤1.00 | ≤0,040 | ≤0,020 | - | ≤1.00 | - | ≤0,030 | Ti6(C+N)~0.50 Nb:0.17 |
430 | 1Cr17 | ≤0.12 | 16.00-18.00 | - | ≤1.0 | ≤0,040 | ≤0,030 | - | ≤1.0 | - | - | - | |
444 | S44400 | ≤0,025 | 17.50-19.50 | 1 | ≤1.00 | ≤0,040 | ≤0,030 | 1.75-2.5 | ≤1.00 | - | 0.035 | Ti+Nb:0.2+4(C+N)~0.80 | |
446 | S44600 | ≤0.20 | 23.00-27.00 | 0.75 | ≤1.5 | ≤0,040 | ≤0,030 | 1.50-2.50 | ≤1.00 | - | ≤0.25 | - | |
Martensit | 410 | 1Cr13 | 0.08-0.15 | 11.50-13.50 | 0.75 | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - |
410S | * | ≤0,080 | 11.50-13.50 | 0.6 | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
416 | Y1Cr13 | ≤0.15 | 12.00-14.00 | 3) | ≤1.25 | ≤0,060 | ≥0.15 | - | ≤1.00 | - | - | - | |
420 | 2Cr13 | ≥0.15 | 12.00-14.00 | - | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
420J2 | 3Cr13 | 0.26-0.35 | 12.00-14.00 | - | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
431 | 1Cr17Ni2 | ≤0.20 | 15.00-17.00 | 1.50-2.50 | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤0.80 | - | - | - | |
440C | 11Cr17 | 0.95-1.20 | 16.00-18.00 | - | ≤1.00 | ≤0,040 | ≤0,030 | 0.75 | ≤1.00 | - | - | - | |
PH | 630 | 17-4PH | ≤0.07 | 15.00-17.50 | 3.00-5.00 | ≤1.00 | ≤0,035 | ≤0,030 | - | ≤1.00 | 3.00-5.00 | - | Nb 0.15-0.45 |
631 | 17-7PH | ≤0.09 | 16.00-18.00 | 6.50-7.50 | ≤1.00 | ≤0,035 | ≤0,030 | - | ≤1.00 | ≤0,50 | - | Al 0,75-1,50 | |
632 | 15-5PH | ≤0.09 | 14.00-16.00 | 3.50-5.50 | ≤1.00 | ≤0,040 | ≤0,030 | 2.00-3.00 | ≤1.00 | 2.5-4.5 | - | Al 0,75-1,50 |
Katerangan
321 stainless steel strip mangrupakeun tipe austenitic stainless steel kalawan eusi karbon lemah sareng lalawanan korosi alus mun loba lingkungan corrosive.321 nawarkeun weldability alus teuing, machinability alus sarta sipat fabrikasi beredar.
321 strip stainless steel ilahar dipaké dina industri kimia, bubur jeung industri kertas, laut jeung industri rékayasa lepas pantai ogé dina industri dahareun jeung inuman.
321 strip stainless steel ogé ngabogaan tingkat luhur lalawanan ka klorida stress korosi cracking na pitting.Éta ogé tahan ka asam hidroklorat dina suhu luhur nepi ka 250 ° C (480 ° F).
Fitur
Résistansi korosi anu hadé: 321 strip stainless steel gaduh résistansi korosi anu langkung saé tibatan 304 sareng 316 jinis stainless steel, anu ngajantenkeun éta cocog pikeun dianggo dina lingkungan korosif.
Weldability alus teuing: 321 strip stainless steel bisa dilas ku sagala métode kaasup arc las (TIG / GTAW), éléktron beam las (EBW / EFW), submerged arc las (SAW) jeung laser beam las (LBIW).
Kakuatan Luhur: Tingkat kakuatan 321 strip stainless steel nepi ka 50% leuwih luhur ti 304 jenis stainless steel sarta nepi ka 80% leuwih luhur ti 316 jenis stainless steel alatan ngaronjat eusi karbon jeung ukuran sisikian austenite.