444/441/409/439/420 Stainless Steel Coil
Katerangan
spésifikasi:
1. Standar: ASTM A240, JIS G4304, EN10088
2. Kelas: 200seri&300seri&400seri
3. Kandel: 0.03mm - 6.0mm
4. rubak: 8mm-600mm
5. Panjang: sakumaha pamundut konsumén '
6. Surface: 2D,2B, BA, Eunteung réngsé, N04, Garis Rambut, Matt finish, 6K, 8K
7.Technology: tiis digambar / tiis digulung / panas digulung
Bahan:
Tipe | Kelas | Kelas | Komponén Kimia% | ||||||||||
C | Cr | Ni | Mn | P | S | Mo | Si | Cu | N | Lain | |||
Austenitik | 201 | SUS201 | ≤0.15 | 16.00-18.00 | 3.50-5.50 | 5.50–7.50 | ≤0,060 | ≤0,030 | - | ≤1.00 | - | ≤0.25 | - |
202 | SUS202 | ≤0.15 | 17.00-19.00 | 4.00-6.00 | 7.50-10.00 | ≤0,060 | ≤0,030 | ≤1.00 | - | ≤0.25 | - | ||
301 | 1.4310 | ≤0.15 | 16.00-18.00 | 6.00-8.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | ≤0.10 | - | |
304 | 1.4301 | ≤0.07 | 17.00-19.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
304L | 1.4307 | ≤0,030 | 18.00-20.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
304H | 1.4948 | 0.04-0.10 | 18.00-20.00 | 8.00-10.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
309 | 1.4828 | ≤0.20 | 22.00-24.00 | 12.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
309S | * | ≤0.08 | 22.00-24.00 | 12.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | - | |
310 | 1.4842 | ≤0.25 | 24.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1,50 | - | - | - | |
310S | * | ≤0.08 | 24.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1,50 | - | - | - | |
314 | 1.4841 | ≤0.25 | 23.00-26.00 | 19.00-22.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | 1.50-3.00 | - | - | - | |
316 | 1.4401 | ≤0.08 | 16.00-18.50 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | - | - | |
316L | 1.4404 | ≤0,030 | 16.00-18.00 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | - | - | |
316Ti | 1.4571 | ≤0.08 | 16.00-18.00 | 10.00-14.00 | ≤2.00 | ≤0,045 | ≤0,030 | 2.00-3.00 | ≤1.00 | - | 0.1 | Ti5(C+N)~0,70 | |
317 | * | ≤0.08 | 18.00-20.00 | 11.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | 3.00-4.00 | ≤1.00 | - | 0.1 | - | |
317L | 1.4438 | ≤0.03 | 18.00-20.00 | 11.00-15.00 | ≤2.00 | ≤0,045 | ≤0,030 | 3.00-4.00 | ≤1.00 | - | 0.1 | - | |
321 | 1.4541 | ≤0.08 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Ti5(C+N)~0,70 | |
321H | * | 0.04-0.10 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Ti5(C+N)~0,70 | |
347 | 1.4550 | ≤0.08 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Nb≥10*C%-1.10 | |
347H | 1.494 | 0.04-0.10 | 17.00-19.00 | 9.00-12.00 | ≤2.00 | ≤0,045 | ≤0,030 | - | ≤1.00 | - | - | Nb≥10*C%-1.10 | |
Duplex | 2205 | S32205 | ≤0.03 | 22.0-23.0 | 4.5-6.5 | ≤2.00 | ≤0,030 | ≤0,020 | 3.0-3.5 | ≤1.00 | - | 0.14-0.20 | |
2507 | S32750 | ≤0.03 | 24.0-26.0 | 6.0-8.0 | ≤1.20 | ≤0,035 | ≤0,020 | 3.0-5.0 | ≤0.80 | 0.5 | 0.24-0.32 | ||
Ferrite | 409 | S40900 | ≤0.03 | 10.50-11.70 | 0.5 | ≤1.00 | ≤0,040 | ≤0,020 | - | ≤1.00 | - | ≤0,030 | Ti6(C+N)~0.50 Nb:0.17 |
430 | 1Cr17 | ≤0.12 | 16.00-18.00 | - | ≤1.0 | ≤0,040 | ≤0,030 | - | ≤1.0 | - | - | - | |
444 | S44400 | ≤0,025 | 17.50-19.50 | 1 | ≤1.00 | ≤0,040 | ≤0,030 | 1.75-2.5 | ≤1.00 | - | 0.035 | Ti+Nb:0.2+4(C+N)~0.80 | |
Martensit | 410 | 1Cr13 | 0.08-0.15 | 11.50-13.50 | 0.75 | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - |
410S | * | ≤0,080 | 11.50-13.50 | 0.6 | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
420 | 2Cr13 | ≥0.15 | 12.00-14.00 | - | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
420J2 | 3Cr13 | 0.26-0.35 | 12.00-14.00 | - | ≤1.00 | ≤0,040 | ≤0,030 | - | ≤1.00 | - | - | - | |
PH | 630 | 17-4PH | ≤0.07 | 15.00-17.50 | 3.00-5.00 | ≤1.00 | ≤0,035 | ≤0,030 | - | ≤1.00 | 3.00-5.00 | - | Nb 0.15-0.45 |
631 | 17-7PH | ≤0.09 | 16.00-18.00 | 6.50-7.50 | ≤1.00 | ≤0,035 | ≤0,030 | - | ≤1.00 | ≤0,50 | - | Al 0,75-1,50 | |
632 | 15-5PH | ≤0.09 | 14.00-16.00 | 3.50-5.50 | ≤1.00 | ≤0,040 | ≤0,030 | 2.00-3.00 | ≤1.00 | 2.5-4.5 | - | Al 0,75-1,50 |
Inpo dasar
Kami ngadamel sareng ngarancang cadar ieu saluyu sareng standar global sareng domestik.Lambaran ieu awét pisan sareng awét sareng tiasa diaksés dina bentuk sareng ukuran anu béda.Konsumén di sakuliah dunya mésér cadar kelas ieu dina bentuk sareng jinis anu béda-béda kusabab fitur sareng pasipatanana anu saé.
Fitur tina lambaran stainless steel ngawengku:
Formability sedeng
Ningkatkeun résistansi ngarayap
Résistansi oksidasi anu langkung luhur
lalawanan korosi alus teuing
kakuatan tensile tinggi
Daya tahan
Kamampuhan gawé
Lambaran ieu didamel nganggo bahan baku kualitas luhur sareng téknologi pang anyarna anu dianggo pikeun nyiptakeun ukuran sareng panjang anu akurat tina lambaran ieu.Salian ti éta, aya sababaraha tés sareng pamariksaan anu dilakukeun anu kalebet:
Tes flattening
Tes flaring
Inspeksi pihak katilu
Tes radiografi
Uji ultrasonik
Pikeun sadaya tés ieu, sertipikat tés anu béda disatujuan anu ditawarkeun ka konsumén anu ngabuktikeun kualitas lembar.Tungtungna, Lembar AISI / SS 441 dibungkus ku panyiri dina bahan bungkusan kualitas luhur sareng dikirimkeun ka konsumén masing-masing di sakuliah dunya.